Casting Defects Handbook: Copper & Copper-Base Alloys

Casting Defects Handbook: Copper & Copper-Base Alloys

List Price $80.00
Member Price $60.00
Corporate Member Price $40.00

Product No. GM10CU; ISBN: 978-0-87433-365-7

Softcover; 4½ x 7; 89 pages

Technical Editor: David Neff; Published 2010: Reprinted 2024.

In Casting Defects Handbook: Copper & Copper-Base Alloys, many of the common types of casting defects encountered in the production of copper base alloy castings in both sand and permanent mold processes are presented. These defects are categorized by type with possible causes and, in some cases, prevention techniques.

The material is presented in an easy-to-review format suitable for foundry floor operators, as well as process engineers, metallurgists and quality control personnel. The book provides a comprehensive visual atlas of the more common casting defects encountered by copper base foundry personnel, and provides a tool for quick identification. It can also be used to address possible causes and to establish corrective actions.

Table of Contents:

  • 1. Broken or Cracked Castings
  • 2. Scars, Seams, Plates and Flow Marks
  • 3. Expansion Defects
  • 4. Sand Molding Defects
  • 5. Misruns and Coldshuts
  • 6. Hot Tearings
  • 7. Gas Defects
  • 8. Shrinkage Defects
  • 9. Metal Penetration
  • 10. Inclusion Defects

Keywords: defects, copper, quality, sand molding, cracks, hot tears, shrinkage, inclusions