Casting Defects Handbook: Aluminum & Aluminum Alloys

Casting Defects Handbook: Aluminum & Aluminum Alloys

List Price $80.00
Member Price $60.00
Corporate Member Price $40.00

Product No. GM11AL, ISBN: 978-0-87433-366-4

Softcover, 4½ x 7, 161 pages

Technical Editor: David Neff; Published 2011

In Casting Defects Handbook: Aluminum & Aluminum Alloys, many of the common types of casting defects encountered in the production of aluminum alloy castings are presented. These defects are categorized by production method: sand-casting, permanent mold, high pressure diecasting, low pressure, investment, plaster and lost foam, with possible causes and, in some cases, prevention techniques listed.

The material is presented in an easy-to-review format suitable for foundry floor operators, as well as process engineers, metallurgists and quality control personnel. The book provides a comprehensive visual atlas of the more common casting defects encountered by aluminum foundry personnel, and provides a tool for quick identification. It can also be used to address possible causes and to establish corrective actions.

Table of Contents

  1. Sand Casting
        Sand, Core and Molding Practice Related
        Metallurgically Related
  2. Permanent Mold
        Surface and Casting Shape Defects
        Gas Defects
        Shrinkage Defects
        Inclusion Defects
  3. High Pressure Diecasting
        Diecasting – Process Related
        Diecasting – Metallurgically Related
  4. Low Pressure Casting
  5. Investment Casting
        Shell and Pouring Defects
        Metal-Related Defects
  6. Plaster Casting
  7. Lost Foam Casting
        Pattern Defects
        Coatings/Sand Defects

Keywords: defects, aluminum, quality, permanent mold, diecasting, investment casting, plaster casting, lost foam casting, gas defects, shrinkage, inclusions